Chemical Composition
Chemical Element | % Present |
---|---|
Iron (Fe) | 0.00 - 0.05 |
Titanium (Ti) | 0.00 - 0.20 |
Magnesium (Mg) | 0.00 - 0.20 |
Zinc (Zn) | 0.00 - 0.15 |
Tin (Sn) | 0.00 - 0.20 |
Hydrogen (H) | 0.90 - 1.40 |
Lithium (Li) | 1.20 - 1.80 |
Molybdenum (Mo) | 0.80 - 1.40 |
Selenium (Se) | 0.00 - 0.25 |
Ti plus Nb (Ti+Nb) | 0.00 - 0.05 |
Yttrium (Y) | 0.00 - 0.10 |
Copper (Cu) | 1.80 - 2.70 |
Aluminium (Al) | Balance |
Applications
- Aerospace & defence components
Characteristics
- Good machinability
- Fair resistance to atmospheric attack
Additional Information
Mechanical Properties
Diameter (mm) | Proof Strength | Tensile Strength | Elongation |
---|---|---|---|
Up to & incl. 10 | 320 Min | 400 Min | 5% Min |
Over 10 up to & incl. 100 | 340 Min | 420 Min | 7% Min |